Incomplete root penetration (bridging) on a T section


By Frédéric REVERDY, Business Development Manager in M2M

Detection of an incomplete root penetration (bridging) on a T section. The component is defined on GEKKO. This creates a profile in the Sscan view. GEKKO can represent the data taking into account the reflexion off the backwall (probe is on the top left here). We can identify easily all the echoes and size properly our defect.

#Tsection #Tjoint #Fillet #weld #joint